شکستگی پیچ دستگاه قالب گیری تزریق

اوت 17, 2021

در پیچ fracture temperature is also related, اما نادر است, تقریباً تمام پیچ های خود از سختی ضعیف است, یا از پیچ برای مدت طولانی استفاده شده است, پیچ را مرمت کنید!

در قالب گیری تزریقی مواد are rough. مثلا, اضافه کردن GF [فیبر شیشه ای] مواد قالب گیری تزریق گرانترین پیچ و ماشین است! This injection molding material has poor fluidity and requires a fast rate of fire! If you don’t master it well, the lighter has the rocket head and the inverse ring break, and the heavy one breaks the screw into knots! Screw breakage can be prevented. When using raw materials to add GF, if the machine is stopped for more than 3 دقایق, it is necessary to clean the مواد خام in the barrel when the machine is turned on. It is best to use PP with higher viscosity to clean the screw to prevent the decomposition of the injection molding raw materials to wrap the screw and rocket head. .

When cleaning, the rotation speed is reduced, so that the injection molding materials are fully melted when heated and rotated. The cleaning screw is the best for pin-point molds to prevent the glue channel from sticking to the static template. Use hot materials to start production!

screw fracture

When the work order is full, متوقف کردن تزریق دستگاه and complete the work, and the mass-produced product is enough. Stop the machine and clean the screw immediately, so that all the residual injection materials of the screw are discharged, and then use PP or clean the injection material of the screw.

 

Process problems, back pressure and screw breakage are also related! If the back pressure is too large, when feeding, the post-screw work force increases, which can also cause the screw to break! دستگاه های رنگ آمیزی پلاستیک به پنج دسته تقسیم می شوند

The end point of the plastic injection cannot be zero, especially with a high-speed injection machine [accumulated gas] shooting can easily damage the rocket head! The projected residual volume should be controlled well. Remember, the most important thing is that the holding pressure time must be adjusted to zero after manual injection to prevent the end point of the injection from being zero!

 

The molding temperature must be controlled well. When starting up, pay attention to loosening and retreating before shooting, because when there is no loosening, there is a raw material package at the rocket head. If the material is washed or shot directly, it can directly cause the rocket head to break and the reverse ring to break. Remember to loosen it and then Shoot to separate the injection material of the rocket head from the rocket head! !

 

Remember that no matter what injection material is used, if the machine stops and does not produce, all the remaining injection material must be discharged to prepare for the next production!

اگر سوالی دارید در مورد پیچ,لطفا در صورت تمایل بپرسید تیم FLYSE,ما بهترین خدمات را به شما ارائه خواهیم داد!

Whatsapp / Wechat 008618958305290

دسته بندی و برچسب ها:
وبلاگ , ,

شاید شما هم دوست داشته باشید

  • محصولات ویژه

    ماشینهای قالب گیری تزریقی با سرعت بالا
    دستگاه های قالب گیری تزریقی PET
    دستگاه های قالب گیری تزریق PVC
    ماشین آلات قالب تزریق دو رنگ

  • با ما تماس بگیرید

    سیار:+86.18368497929
    وچت: +86.18368497929
    واتساپ: +86.18368497929
    وب:www.yongjiangimm.com
    پست الکترونیک:yongjiangimm@gmail.com

  • سرویس
    Yongjiang تامین کننده قابل اعتماد شما! اسکن کنید, برای بهتر صحبت کنید